DESIGNING INGREDIENTS OF BTX FLASH-REDUCED PROPELLANT WITH A HIGH PVC CONTENT

  • Duy Binh Le Institute of Propellant and Explosives, General Department of Defence Industry
Keywords: Propellant, BTX, chemical stability, PVC, thermochemical coefficient, chlorine content, ingredients

Abstract

Based on experiments, it was researched to determine the kind of pyroxylin and the effect of flash-reduced additives (PVC) on the quality of BTX propellant. Therefore, it designed ingredients for the research and manufacture of propellant of BTX with high PVC content. The results show that the kind of pyroxylin used type BA with a high nitrogen content (about 13.26% N). The flash-reduced additive is the PVC with chlorine content at 61-65%
and the thermochemical coefficient of PVC is about -(2 ± 0.5) kcal/(kg x %). When using PVC with the above properties the chemical stability of the propellant is high. At that time, the ingredients of BTX flash-reduced propellant with a high PVC content are determined to be about 77% Pi-BA; 20% PVC; 1.38% DPA; 0.35% ethyl-alcohol; 0.15% ethyl-ether; 1.1% moisture and about 0.02% graphite (addition).

điểm /   đánh giá
Published
2025-05-19
Section
SCIENTIFIC RESEARCH