Synthesis of Wollastonite mineral by two stage reaction: hydrothermal and calcination reaction from rice hush and portlandite
Keywords:
hydrothermal reaction, rice hush, Wollastonite.
Abstract
This research presents the synthesis process of Wollastonite mineral by two stage reaction, hydrothermal and calcination, using Vietnam rice husk and portlandite. The rice husk ash after burning was batch mixed with Ca(OH)2 with the Ca/Si molar ratio of 1.0, followed by hydrothermal treatment at 180oC to obtain Xonotlite mineral. The obtained Xonotlite mineral was calcined at 900oC for 5 hours to form a Wollastonite owning fibre shape interlocked together to form an interconnected porous structure with a pore size of 1~2 µm, which could be suitable for industrial application.
điểm /
đánh giá
Published
2022-08-29
Section
KHOA HỌC KỸ THUẬT VÀ CÔNG NGHỆ